Lithium Niobate(LiNbO3) Crystal is widely used as frequency doublers for wavelength > 1 mm and optical parametric oscillators (OPOs) pumped at 1064 nm as well as quasi-phase-matched (QPM) devices. Due to its large Electro-Optic (E-O) and Acousto-Optic (A-O) coefficients.

We supplies high quality and large size LiNbO3 crystals for laser frequency doublers, OPOs and quasi-phase-matched doublers, as well as waveguide substrate and SAW wafers. High quality LiNbO3 finished components with aperture of (2 - 15) x (2 - 15) mm2 and length up to 50 mm for frequency doublers and optical parametric oscillators (OPOs), 50x50x1 mm3 or Dia. 3" x 1 mm LiNbO3 substrate for waveguide optics, and Dia. 3" optical wafers are available with high volume and at low price.

Physical Properties  
Crystal Structure Trigonal, space group R3c
Cell Parameters a = 0.515, c = 13.863, Z = 6
Melting Point 1255 +/-5
Curie Point 1140 +/-5
Mohs Hardness 5
Density 4.64 g/cm3
Absorption Coefficient ~ 0.1%/cm @ 1064 nm
Solubility insoluble in H2O
Relative Dielectric Constant eT11/e0: 85
eT33/e0: 29.5
Thermal Expansion Coefficients at 25癈 ||a, 2.0 x 10-6/K @ 25
Thermal Conductivity 38 W /m /K @ 25
Optical Properties  
Transparency Range 420 - 5200 nm
Refractive Indices ne = 2.146, no = 2.220 @ 1300 nm
ne = 2.156, no = 2.322 @ 1064 nm
ne = 2.203, no = 2.286 @ 632.8 m
Optical Homogeneity ~ 5 x 10-5 /cm
Sellmeier Equations( l in mm) no2(l) = 4.9048+0.11768/(l2 - 0.04750) - 0.027169 l2
ne2(
l) = 4.5820+0.099169/(l2- 0.04443) - 0.021950 l2
NLO Coefficients d33 = 34.4 pm/V
d31 = d15 = 5.95 pm/V
d22 = 3.07 pm/V
Electro-Optic Coefficients gT33 = 32 pm/V, gS33 = 31 pm/V
gT31 = 10 pm/V, gS31 = 8.6 pm/V
gT22 = 6.8 pm/V, gS22 = 3.4 pm/V
Half-Wave Voltage, DC
Electrical field ||z, light ^ z
Electrical field ||x or y, light || z
3.03 KV 4.02 KV
Damage Threshold 200 MW/cm2 (10 ns)
Efficiency NLO Coefficients deff=5.7pm/V or~14.6xd36(KDP) for frequency doubling 1300 nm;
deff=5.3pm/V or~13.6xd36(KDP) for OPO pumped at 1300nm;